Abstract

Impulse and dc breakdown strengths of 4 /spl mu/m thick poly-p-xylylene (PPX) films were 5.9 and 4.1 MV/cm, respectively. They were independent of temperature in the temperature range from /spl minus/60 to 60/spl deg/C. dc prestressing for a long time (t/sub p/=60 s) reduced impulse breakdown strength for both the same and the opposite polarity. But dc prestressing for a short time (t/sub p/ >

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.