Abstract

To improve bioactivity of gradient bioceramic coating, the coating with two kinds of rare earth oxide was produced by wide band laser cladding technique. As the experimental results, whichadded0.6wt.% La2O3 fixedly, and increased the addition amount of the CeO2, when the addition of CeO2fulfill 0.4wt.%, the amount of HA-β-TCP is the largest in this experiment. Soaking the specimens in SBF for 14 days, the coating blended 0.6wt% La2O3 and 0.4wt% CeO2, then a great quantity of Ca-P white particles can be found on coating, which confirmation this bioceramic coating is of best bioactivity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.