The preferred orientation of hydroxyapatite Ca10(PO4)6(OH)2 (HAp) crystallites at the interface bone-implant in sheep tibia bones has been measured with the neutron 2-axis diffractometer D20 at the Institut Max von Laue-Paul Langevin, extracted 60 days after implantation. The implant has two faces, one coated and one non-coated with plasma-sprayed HAp (80 µm). We probed the samples with a spatial resolution of 0.5 mm started from the interface in order to inspect the reorganisation of the HAp crystallite distribution after implantation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.