Abstract
Three specimens with different initial δ phase contents have been used to study the tensile deformation and fracture characteristics of the delta-processed Inconel 718 alloy at elevated temperatures by tensile tests at 950 °C. The results indicated that the tensile stress–strain curves of the three specimens were the elastic-uniform plastic curves, and there were two deformation processes during the uniform plastic deformation stage of the delta-processed specimens. The strain hardening exponent in the first deformation process was higher than that in the second process, and the value of the strain hardening exponent increased as the content of δ phase increased. In addition, the plasticity of the specimen at elevated temperatures decreased as the content of δ phase increased. However, the fracture mechanisms for all the specimens were all microvoid coalescence ductile fracture, and the δ phase and carbide were the nucleuses for the formation of micropores. The elongation for the specimen with 8.21% pre-precipitated δ phase was still as high as 80%. Thus, delta-processed Inconel 718 alloy presented excellent high-temperature plasticity.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.