Abstract
Sputtering nanocrystalline coating was prepared on a nickel-based single-crystal superalloy N5. The oxidation behavior of the superalloy substrate and its nanocrystalline coating was investigated at 900–1100°C. Results indicated that the nanocrystalline coating enhanced the oxidation and scale spallation resistance of the single-crystal superalloy. Elements interdiffusion has not occurred between the substrate and coating. Refractory element, Ta, inherently contained in N5, had a significant effect on the scale microstructure and oxidation behavior of both the single-crystal superalloy substrate and its sputtering nanocrystalline coating.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.