Abstract

AbstractPoly(diphenylacetylene)s having various silyl groups are soluble in common solvents, from whose membranes poly(diphenylacetylene) membranes can be obtained by desilylation. The oxygen permeability coefficients of the desilylated polymers are quite different from one another (120–3300 barrers) irrespective of the same polymer structure. When bulkier silyl groups are removed, the oxygen permeability increases to larger extents. Poly[1‐aryl‐2‐p‐(trimethylsilyl)phenylacetylene]s are soluble in common solvents, and afford free‐standing membranes. These Si‐containing polymer membranes are desilylated to give the membranes of poly[1‐aryl‐2‐phenylacetylene]s. Both of the starting and desilylated polymers show very high thermal stability and high gas permeability. 1‐Phenyl‐2‐p‐(t‐butyldimethylsiloxy)phenylacetylene polymerizes into a high‐molecular‐weight polymer. This polymer is soluble in common organic solvents to provide a free‐standing membrane. Desilylation of this membrane yields a poly(diphenylacetylene) having free hydroxyl groups, which is the first example of a highly polar group‐carrying poly(diphenylacetylene). The P/P and P/P permselectivity ratios of poly(1‐phenyl‐2‐p‐hydroxylphenylacetylene) membrane are as large as 47.8 and 45.8, respectively, while keeping relatively high P of 110 barrers. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 5028–5038, 2006

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.