LiNO3 was used as a shield in the preparation of single crystalline ZnO particles by a spray pyrolysis process in order to prevent agglomeration and enhance the crystallinity of the ZnO. LiNO3 was added to a precursor solution of zinc acetate dihydrate prior to its atomization by means of an ultrasonic transducer. Agglomerate-free particles having a mean particle size of 26 nm were successfully obtained after washing the product. X-ray diffractometry, field-emission scanning electron micrograph and transmission electron micrograph data indicate that the size and morphology of ZnO were strongly influenced by the operating temperature used and the residence time of the particle in the reactor.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.