Abstract
In this work, for the first time, single-phase potassium-sodium niobate powder with a primary particle size of 0.3-3.1 μm was synthesized in a water vapor medium at a temperature of 260oC and a pressure of 4.69 MPa. Two different techniques, the traditional one and laser stereolithography, were applied to produce powder-based ceramics with a density reaching 80-85% of the theoretical value. A set of the most important piezoelectric characteristics was studied for the prepared ceramics. The obtained preliminary results indicated the prospect of improving the phase, structural, and piezoelectric properties of potassium-sodium niobate ceramics by controlling the parameters of powder synthesis in water vapor and enhancement of the sintering conditions. Keywords: piezoelectric ceramics, complex oxide synthesis, potassium-sodium niobite, laser stereolithography.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.