Abstract

Microstructured ZnO have been synthesized by a simple hydrothermal approach, using ZnCl2as the zinc source and N2H4·H2O as the amine precursor in water-ethylene glycol solution at 120 °C for 8 h. The X-ray diffractrometer pattern indicates the pure phase formation of ZnO. Scanning electron microscope images show that the aspect ratio of the ZnO microrod increases by the amount of N2H4·H2O ranging from 0.5 to 1mL, but continuing to 3ml, the aspect ratio of the ZnO microrods decreases. Moreover, the optical band gaps calculated through UV spectroscopy are found to increase from 2.94 (±0.02) to 3.0 (±0.02) eV for samples synthesized at different amounts of hydrazine hydrate ranging from 0.5 to 1mL, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.