Abstract
In this work pure and transition elements (Ni and Cu) doped Zinc Oxide is prepared. All the samples were prepared through chemical co-precipitation method, by using sulfates of metallic precursors. We have doped pure ZnO with Ni and Cu by 3% by weight concentration. Further the structural, Crystallite size and band gap approximation studies were performed by utilizing X-ray diffraction and spectroscopic techniques respectively. X-ray diffraction (XRD) result indicates that the sample possess a crystalline Wurtzite single phase. Crystallite size is in 19-30 nm range. PL characterization gives optical band gap that is 2.65-3.0 2 eV. FTIR gives the molecular band present in the samples. UV-Vis shows red shift in peak wavelength.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.