Abstract

Pt-Pd bimetallic nanoparticles were synthesized on TiO2 support on the planar substrate as well as on high surface area SiO2 gel by atomic layer deposition to identify the catalytic performance improvement after the formation of Pt-Pd bimetallic nanoparticles by surface analysis techniques. From X-ray absorption near edge spectra of Pt-Pd bimetallic nanoparticles, d-orbital hybridization between Pt 5d and Pd 4d was observed, which is responsible for charge transfer from Pt to Pd. Moreover, it was found from the in situ grazing incidence X-ray absorption spectroscopy study that Pt-Pd nanoparticles have a Pd shell/Pt core structure with CO adsorption. Resonant photoemission spectroscopy on Pt-Pd bimetallic nanoparticles showed that Pd resonant intensity is enhanced compared to that of Pd monometallic nanoparticles because of d-orbital hybridization and electronic states broadening of Pt and Pd compared monometallic catalysts, which results in catalytic performance improvement.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.