Abstract
Purpose: This study was designed to measure surface softness of a new contact lens material (NCLM) with biologically inspired water gradient surface after 30 days of daily wear (DW) and 6 nights/7 days extended wear (EW). These values were compared with fresh lenses and other contact lens benchmarks.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.