Abstract In preparation for synthesizing LaCoO3, gel was prepared by adding citric acid to the aqueous solution of La(NO3)3·6H2O and Co(NO3)2·6H2O. The infrared spectrum indicates that the gel prepared with 0.007 mol of citric acid is the mixture of LaCo(C6H5O7)(NO3)3, lanthanum nitrate, and cobalt nitrate, while the gel prepared with 0.011 mol of citric acid is LaCo(C6H5O7)2. Perovskite-type LaCoO3 was obtained by firing the gel above 600°C. The LaCoO3 surface was characterized by X-ray photoelectron spectroscopy and with respect to the catalytic activity of CO oxidation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Preprints of Annual Meeting of The Ceramic Society of Japan<br> Preprints of Fall Meeting of The Ceramic Society of Japan
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.