Abstract

The polycrystalline CaBi2Nb2O9 ceramics with the addition of B2O3 can realize a large d33 of 20.4 pC N−1 and an ultra-high electrical resistivity of 1.4 × 107 Ω cm (at 600 °C), while still retaining a high TC of 958 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.