In this paper, the slag-metal equilibrium experiments were performed to investigate the effect of TiO2 concentration in the slag and basicity (R=wt%CaO/wt%SiO2) on the sulphur distribution ratio (Ls) between CaO-SiO2-TiO215%Al2O3-8%MgO slag and carbon-saturated iron at 1773 K. Sulphide capacities (Cs) were calculated based on the sulphur distribution ratio. The sulphur distribution ratio and sulphide capacity of CaO-SiO2-TiO2-15%Al2O3-8%MgO stage increase with increase of basicity and with decrease TiO2 concentration in the slag. The relationship between sulphide capacity of CaO-SiO2-TiO2-15%Al2O3-8%MgO slag and optical basicity was also investigted. The experimental results are useful for smelting vanadium titaniferrous magnetite of blast furnace.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.