Abstract

In the course of the milling experiments with the difficult-to-machine material 3Cr-1Mo-1/4V steel, we have found the substance of the adhering disrepair. In addition, we forecast the predominant capability of the waved-edge milling insert with complex 3-D grooves by the synthetically blurry judgement. Eventually, we give the mathematical model between the milling temperature and the maximal adhering disrepair depth of the rake face, and analyze the rule that the milling temperature affects the adhering disrepair. What’s more, we testify the predominant capability of the waved-edge milling insert.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.