Abstract

AbstractOur work presents results on human plasma protein adsorption onto a polyacrylic acid (PAA) film prepared via surface wave plasma (SWP) induced graft polymerization. The PAA film prepared in this manner is characterized by a carboxyl functional group and a constant contact angle in water of 35°. The adsorption kinetics of human plasma fibrinogen (HPF) and human serum albumin (HSA) proteins were measured by in-situ UV-ATR spectroscopy. The free energy of adsorption on PAA treated as well as untreated surfaces was −28 kJ M−1 and −22 kJ M−1 for HPF and HSA, respectively, regardless of surface chemistry. We determined that 14 μM and 6 μM HPF concentrations are enough to cover half of the maximum possible of surface coverage on silica and PAA film, respectively. HSA protein concentrations of 154 μM and 118 μM are enough to cover half of the maximum accessible surface of silica and PAA film, respectively. For surface treatment of implants with PAA polymer and protein, the necessary protein concentration for effective surface coverage should be known.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.