Abstract

It was found that Co50Ni20Gax (x=0–40) melt-spun ribbons were ferromagnetic, but Co50Ni20Ga40 melt-spun ribbon was paramagnetic at room temperature. The addition of Ga to Co–Ni melt-spun ribbon significantly reduced the saturation magnetization. It was also found that the Curie temperature of the β phase in Co50Ni20Gax (x=20–30) melt-spun ribbons was around 300K and that of the β phase in Co50Ni20Ga40 melt-spun ribbon was 110K. Unlike the other Co–Ni–Ga melt-spun ribbons, Co50Ni20Ga30 melt-spun ribbon exhibited a coercivity of 1.0kOe after annealing at 773K for 1h.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.