Superconducting fibers have drawn great attention because of the latent prospect for applications. Fibers of superior quality were obtained by means of the laser-heated pedestal growth (LHPG) method. For LHPG method a fine laser beam is focused at the “source rod” made of raw material so that a small molten zone is formed on its upper end. Then a seed crystal is introduced into the melt and drawn from it to grow crystalline fibers. In this paper the structure of bismuth based Bi-Sr-Ca-Cu-O and Bi-Pb-Sr-Ca-Cu-O superconducting fibers prepared by LHPG is reported. The values of Tc for the two kinds of fibers are 85k and 108k respectively. The critical current density Jc can reach 5150A/cm2. The diameters of fibers are ranged from 35μm-200μm. The thin fibers are flexible.Fig.1 shows the transition region between the source rod (R) and the LHPG fiber (G). It indicates that the source crystal first melts and then recrystallizes along a certain cry stenographic direction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.