Abstract

Application of electroplastic deformation (EPD) by rolling to bulk long-sized samples of Ti-50.7 at.%Ni alloy allows increasing of the deformation strain without macrofailure by 1.5 to 3 times in comparison to cold rolling without electrical current application. Structure formation and functional properties were studied after various EPD regimes: current density (84 to 168 А/mm2) and impulse duration (80 and 160 ms). When the stage of mixed nanocrystalline and amorphous structure formation is reached as a result of EPD, a post-deformation annealing at 400 °С leads to a nanocrystalline structure formation in austenite and highest recovery stress values generation by the martensite.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.