Abstract
This work investigates the evolution of the crystal structure of the topologically closed packed orthorhombic P phase precipitate in a Re-containing Ni-based single crystal superalloy during thermal exposure. The P phase is formed with a thin needle morphology. The precipitate is formed from the matrix with an initial complex atomic arrangement which continues to evolve during the process of thermal exposure. Based on the experimental evidence of this study and the theoretically predicted structure reported in the literature, a mechanism of the structural transformation is proposed. The initial structure is composed of a parallelogram (P) atomic arrangement configuration, which gradually evolve into a rectangle (R) atomic arrangement configuration in the [100]P projection. In the [010] projection, the initial structure is composed of alternating rows of a larger parallelogram (P') and a larger rectangle (R') configurations, which gradually evolve into an intricate structure of P'-R' along the length [001]P direction and P'P'-R'R' along the transverse [100]P direction. The initial structure is formed for its structural similarities to the γ phase to minimize lattice mismatch. The final structure is evolved over time to conform to its thermodynamically more stable state. The structural evolution is achieved by collective atomic shuffling. These intricate atomic arrangements gives rise to the very faint and highly dense parallel striation lines along the transverse [010]P direction in [100]P view and along the length [010]P direction in [010]P view under transmission electron microscopy observation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.