Abstract

Green synthesis of zinc oxide nanoparticles (ZnO NPs) through simple, rapid, eco-friendly and an economical method with a new haloalkaliphilic bacterial strain (Alkalibacillus sp. W7) was investigated. Response surface methodology (RSM) based on Box-Behnken design (BP) was used to optimize the process parameters (ZnSO4.7H2O concentration, temperature, and pH) affecting the size of Alkalibacillus-ZnO NPs (Alk-ZnO NPs). The synthesized nanoparticles were characterized using UV–visible spectrum, X-ray diffraction (XRD), Scanning electron microscope-energy dispersive X-ray spectroscopy (SEM–EDX), Transmission electron microscopy (TEM), Fourier transform infrared spectroscopy (FTIR) and Zeta potential. The UV–Vis spectrum of ZnO NPs revealed a characteristic surface plasmon resonance (SPR) peak at 310 nm. XRD pattern confirmed the hexagonal wurtzite structure of highly pure with a crystallite size 19.5 nm. TEM proved the quasi-spherical shape nanoparticles of size ranging from 1 to 30 nm. SEM–EDX showed spherical shaped and displayed a maximum elemental distribution of zinc and oxygen. FTIR provided an evidence that the biofunctional groups of metabolites in Alkalibacillus sp.W7 supernatant acted as viable reducing, capping and stabilizing agents.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.