Abstract

The present study investigates the mechanical properties of soft Bangkok clay which was stabilized by ordinary Portland cement and calcium sulfoaluminate-belite (CSAB) cement. The CSAB cement was synthesized by using several types of industrial waste materials such as marble dust waste and flue gas desulfurization gypsum. The raw materials were mixed in designed proportion and calcined at 1,250 °C for 2 hours. The X-ray diffraction patterns suggested the clinker consists of ~58% of ye'elimite and ~35% of belite. The slurry soft Bangkok clay with liquidity index of 1.0, 1.3 and 1.5 was stabilized with ordinary Portland cement and CSAB cement in the range of 5 - 20%. Based on the laboratory study, mechanism of rising unconfined compressive strength results which soft clay stabilized with CSAB cement could observe from Scanning Electron Microscope images.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.