Abstract

Special features of high-temperature oxidation of aluminide coatings (slip-deposited Al – Si and ion-plasma-deposited VSDP-11) on alloy TsNK-7P are considered. The kinetics of the oxidation process, the element composition, and the microhardness of coatings with different thicknesses are described. Results of thermal fatigue tests of alloy TsNK-7P with aluminide diffusion coatings are presented. It is shown that the VSDP-11 coating ensures a higher heat resistance and thermal fatigue strength on alloy TsNK-7P than the Al – Si coating and can replace the latter on turbine vanes of gas compressor units.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.