Sodium ion conductor with the composition of Na4.0Y0.6P0.2Si2.8O9 was prepared using a sol-gel method (polymerized complex method). The homogeneous gel was prepared by dissolving citric acid and ethylene glycol in mixtures of water solutions of metal salts. Drying the gel provides the uniform precursor. The sintered pellet obtained from the precursor had a single crystalline phase of Na5YSi4O12-type structure and exhibited ionic conductivity of 3.7 × 10−2 S/cm at 300 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.