Abstract

"The soft magnetic nanocrystalline powders, alloys (Ni3Fe, 79Ni16Fe5Mo, 77Ni14Fe5Cu4Mo, wt. %) and zinc ferrite, were obtained by dry and wet mechanical alloying and reactive milling, followed by different heat treatments. The powders were characterised by X-ray diffraction, scanning electron microscopy, X-ray microanalysis, differential scanning calorimetry, thermomagnetic and magnetic measurements. The X-ray diffraction shown the progressive new phases formation. The crystallite size is between 18-7 nm depending on materials and milling conditions. The particle size is smaller for wet-mechanical alloying comparing with dry-milling. The thermomagnetic measurement shown the Curie temperature of the alloys. The spontaneous magnetisation of the wet-milled and annealed samples is higher than of the molten alloys. Keywords: mechanical alloying; Ni-Fe-X-Y alloys; soft ferrite; magnetisation; XRD; DSC. "

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.