Abstract

In this study, iPP was injection molded at 180°C, 200°C, and 220°C. According to polarization optical microscopy (POM) results, for a given part, the skin thickness steadily decreases along the flow direction. However, at the same distance from the gate, the skin thickness of the parts molded at lower melt temperature is larger than that molded at higher melt temperature. It is found that flow time (here, the time taken for melt to pass the specific position along the flow direction) and melt temperature are two significant factors leading to this phenomenon, while the gate size is another one. The DSC and WAXD results show that the relative fraction of β-form crystals, for a specific part, decreases along the flow direction, which is mainly determined by flow time. However, for the parts molded at different molding temperatures, the fraction of the β-form crystals is mainly determined by the molding temperature, though this influence is very complex.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.