Abstract

A process was developed for chromate-free passivation of zinc-plated surfaces via formation of conversion silicon-containing coatings on these surfaces. The passivation performed in a solution containing 20–35 g L−1 sodium metasilicate, 0.2–0.5 g L−1 phosphonic acid, 20–30 mL L−1 H2O2, 200–500 mg L−1 saccharine, and 4–10 mg L−1 potassium pyrophosphate at pH 2.0–2.5 and temperature of 18–25°C in the course of 4 min. A warming-up of the solution to 40°C is allowed. The developed silicon-containing passivating coatings on zinc-plated steel details are comparable in corrosion resistance and protective capacity with iridescent chromate coatings, but, in contrast to the latter, sustain a thermal shock without deterioration of their protective characteristics and are more wear resistant.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.