Several intermediate steps were applied before the precursor infiltration and pyrolysis process to improve the infiltration of SiC slurry for promoting the infiltration of SiC slurry into fiber voids. These steps include sonication, popping, electrophoretic deposition, vacuum infiltration and cold isostatic pressing (CIP). The intermediate processes, especially popping and CIP, had a beneficial effect on green density enhancement and improving the homogeneous infiltration of the slurry into fiber fabrics. The density of the SiCfiber/SiCfiller green body was 2.20 g/cm3, which corresponded to 68 % of relative density. The SiCf/SiC composite has a high density of 2.65 g/cm3 after seven PIP cycles.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.