Selective-area atomic layer deposition (ALD) was achieved using poly(methyl methacrylate) (PMMA) films as growth inhibiting mask layers. The PMMA films were prepared from PMMA−toluene solution by spin-coating and patterned by UV lithography through a mechanical mask. The patterned PMMA films were tested in several ALD processes, both noble metals and oxides. The tested noble metal processes were iridium, platinum, and ruthenium, and the oxide processes were Al2O3 and TiO2. Al2O3 was deposited using AlCl3 and H2O and trimethylaluminum (TMA) and H2O. TiO2 was deposited using Ti(OMe)4 and H2O. The growth temperatures were 250−350 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.