Abstract

The scaling behaviors of the dynamic hysteresis in Zr-rich lead zirconate titanate bulk ceramics at various frequency ( f ) and field amplitude ( E 0 ) values, and in different ferroelectric phases, were investigated. The scaling laws of the hysteresis area 〈 A 〉 at fixed temperature take the forms 〈 A 〉 ∝ f 0.16 E 0 and 〈 A 〉 ∝ f 0.01 E 0 0.2 for low frequency and high frequency, respectively. The forms are different from those of the theoretical predictions and other experimental results but are the same for different ferroelectric phases, which implies that the compositions and crystal structures can influence the scaling laws while the different space groups in the rhombohedral phase can not.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.