Abstract

AbstractIn this study, agave fiber/linear medium density polyethylene composites were manufactured by rotational molding. A laboratory scale biaxial machine was used, where the internal air temperature during the processing cycle was measured. Two sizes of agave fibers (50 and 100 mesh) were used separately and mixed together (50/50) at concentrations varying between 0 and 15 wt%. The initial mixtures were obtained by dry blending, rotomolded under different operation conditions (oven temperature, processing cycle time, and rotational speeds), and the final pieces were compared. For each process condition, a complete morphological analysis was performed to relate with mechanical properties in terms of tensile, impact, and flexural strength. The results show that there is an optimum fiber concentration around 10%, and blending fiber sizes gave better tensile properties than using each size alone. POLYM. ENG. SCI., 2012. © 2012 Society of Plastics Engineers

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.