Abstract
In order to analyze the multi-stage forging process of a nickel-based GH4169 superalloy (similar to Inconel 718 alloy) aero-engine turbine disc with high efficiency and accuracy, a modified material constitutive law, grid convergence study, and a combined two-dimensional and three-dimensional finite element simulation technology were used to analyze the thermo-mechanical-coupled stress variation during the turbine disc multi-stage forging process with the general-purpose nonlinear finite element software MSC.Marc. The predicted finite element forging residual stresses were tested and verified with the measurement results by the layer removal method; it was found that the constitutive law combined with heat contact properties between dies and material could be used to accurately predict and analyze the turbine disc forging processes. Based on the predicted precise and comprehensive finite element residual stress distributions, the consequent disc anti-fatigue manufacturing technologies could be optimized and improved greatly, which would guarantee the stable manufacturing quality and excellent performance of the aero-engine turbine disc.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Proceedings of the Institution of Mechanical Engineers, Part G: Journal of Aerospace Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.