Using anatase and flake graphite as starting material, titanium nitride was prepared by carbothermal reduction nitriding method under nitrogen gas pressure 0.05 MPa and flow rate 0.3 m3/h, at 1673K(1400°C).The proportion of nc and nTiO2 are 1.5:1,2.0:1,2.2:1 and 2.5:1. The phase composition and microstructure of titanium nitride were investigated by XRD and SEM. The results show that: titanium nitride can be prepared with anatase and flake graphite by carbothermal reduction nitriding method. When the proportion of nc and nTiO2 is 2.2:1 the quantity of titanium nitride is the most. Because the reacting temperature is low and the contact area of the anatase and flake graphite is small the large grain size and uniform grain size titanium nitride can not be obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.