Abstract

Manganese (Mn) leaching and recovery from low-grade pyrolusite ore were studied using sulfuric acid (H2SO4) as a leachant and pyrolysis-pretreated sawdust as a reductant. The effects of the dosage of pyrolysis-pretreated sawdust to pyrolusite ore, the concentration of sulfuric acid, the liquid/solid ratio, the leaching temperature, and the leaching time on manganese and iron leaching efficiencies were investigated. Analysis of manganese and iron leaching efficiencies revealed that a high manganese leaching efficiency was achieved with low iron extraction. The optimal leaching efficiency was determined to be 20wt% pyrolysis-pretreated sawdust and 3.0 mol/L H2SO4 using a liquid/ solid ratio of 6.0 mL/g for 90 min at 90°C. Other low-grade pyrolusite ores were tested, and the results showed that they responded well with manganese leaching efficiencies greater than 98%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.