Abstract

Early-age cracking continues to be a significant problem for new concrete construction. Two of the major contributors to such cracking are the heat released by cement hydration during the first few days of curing and the autogenous shrinkage that often occurs during the same time frame. In this paper, three potential alternatives for reducing these contributions by modifying the concrete mixture proportions are investigated, namely increasing the water-cement ratio (w/c), using a coarser cement, or replacing a portion of the portland cement with a coarse limestone powder. Each alternative reduces the heat generated per unit volume by either reducing the volumetric cement content or its early-age reactivity, and reduces autogenous shrinkage by increasing the interparticle spacing between grains in the three-dimensional microstructure. These reductions are quantified for paste and mortar systems by measuring their semi-adiabatic temperature rise and autogenous deformation along with measurements of compressive strength to indicate the strength trade-off that will be experienced in reducing the risk of early-age cracking. These mixtures each have the additional advantage that they should result in a cost savings in comparison with an initial (control) mixture.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.