Abstract

Abstract The samarium (III)/(II) and europium (III)/(II) redox potentials in molten lithium chloride were measured using the direct potentiometric method in the temperature range from 923 to 1094 K. Glassy carbon was used as the indifferent working electrode, and the standard chlorine electrode as a reference. The total concentration of rare-earth chlorides dissolved in molten lithium chloride did not exceed 4.5 mol%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.