Abstract

Through flotation recovery of Silver (Ag) from Zinc acid-leaching residue (ZALR) was investigated in this study. The study adopted the single factor and orthogonal test reveal interactions among all considerable influence factors including sodium sulphide (SS) as regulator, ammonium butyl dithiophosphate (ABD) as major collector, GC as minor collector, interaction between ABD and GC, OC as flotation carrier, and pulp density. The experimental results show the flotation of the circuit composited of one rougher, one cleaner, one scavenger and middlings being back to the next rough flotation together is practical way and that the concentrate containing Ag 10890.0g/t, recovery77.43% can be obtained from the residue (Ag grade 340g/t). The optimum roughing flotation process is: the pH value of flotation pulp is 3.0~4.0, the pulp density is about 45wt.%, ABD dosage is 900g/t, GC dosage is 50g/t, OC dosage is 2000g/t, and BK201 dosage is 100g/t.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.