Abstract

To test the null hypothesis that there is no significant difference in the shear bond strength (SBS) and Adhesive Remnant Index (ARI) scores of new vs reconditioned self-ligating brackets. One hundred and twenty permanent extracted bovine teeth were embedded in resin blocks. Three different new and reconditioned self-ligating orthodontic brackets (Smart Clip [3M Unitek]; Quick [Forestadent]; and Damon3MX [Ormco]) were tested. Scanning electron microphotographs of the different new (groups 1, 3, and 5) and reconditioned (groups 2, 4, and 6) bracket bases were taken before starting the experiments. Brackets were then bonded to the teeth using an orthodontic adhesive and were then tested in shear mode using an Instron Universal Testing Machine. ARI scores were then recorded. Statistical analysis was performed to determine significant differences in SBS and ARI Scores. Smart Clip and Damon3MX reconditioned brackets showed significantly lower SBS than did new ones. On the contrary, Quick reconditioned brackets showed significantly higher SBS than did new ones. No significant differences in ARI scores were found after the reconditioning process for the three different brackets tested. The in-office reconditioning procedure alters the SBS of self-ligating brackets, although SBS values still remain clinically acceptable.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.