Abstract

The identification and intensity estimation of some aluminium emission lines have been proposed to perform an on-line quantification of the Al contribution to the laser-welding process of Usibor blanks. This boron steel is protected by an Al-Si coating that is removed by laser ablation before welding. If this process fails to remove Al from the joint surface, its contribution may affect the final properties of the resulting seams, therefore compromising their quality. Experimental tests have been performed, some of them in a real production scenario. They have been analysed and compared to the results of welding test specimens, analysis of the associated tensile properties and fracture locations and seam macrographs. These studies have indicated that on-line quantification of the Al contribution to the process is feasible and that a correlation can be established between the Al content estimated in real-time and the results derived from the off-line tests considered.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.