Abstract

Reactions between 48Sn-52In solder and under bump metallurgies(UBM) such as 100nmTi/8µm Cu and 300nm Al/400nm Ni(V)/400nm Cu have been investigated, and the shear strength of 48Sn-52In solder bumps on each UBM has been evaluated. While intermetallic compounds with two different morphologies were continuously thickened on Ti/Cu with repeating the reflow process, the intermetallics on Al/Ni(V)/Cu spalled into the solder with increasing the number of reflow times. The solder bumps on Ti/Cu exhibited higher shear strength than those on Al/Ni(V)/Cu.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.