Abstract
In this work we report the in situ preparation of fully biobased stereocomplex poly(lactide) (SC-PLA) nanocomposites grafted onto nanocrystalline cellulose (NCC). The stereocomplexation rate by compounding high-molar-mass poly(D-lactide) (PDLA) with comb-like NCC grafted poly(L-lactide) is rather high in comparison with mixtures of PDLA and PLLA. The rapid stereocomplexation was evidenced by a high stereocomplexation temperature (Tc-sc = 145 °C) and a high SC crystallinity (Xc-sc = 38%) upon fast cooling (50 °C/min) from the melt (250 °C for 2 min), which are higher than currently reported values. Moreover, the half-life crystallization time (175-190 °C) of the SC-PLA was shortened by 84-92% in comparison with the PDLA/PLLA blends. The high(er) stereocomplexation rate and the melt stability of the SC in the nanocomposites were ascribed to the nucleation effect of the chemically bonded NCC and the "memory effect" of molecular pairs in the stereocomplex melt because of the confined freedom of the grafted PLLA chains.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.