Abstract

Directional solidification of aluminium-silicon eutectic alloys were carried out in order to investigate the mechanism by which the quench modification takes place. For this purpose a new type of Bridgman furnace was designed which can attain a high temperature gradient and a high interfacial growth velocity up to 1000 μm−1. It is established that the fibrous structure is the result of faceted-non-faceted growth of the coarse silicon particle at high solidification rate. It is observed that refining of the flake structure closely follows the characteristics of normal eutectic.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.