Abstract

There is a need to increase the temperature capability of superalloy turbine disks to allow higher operating temperatures in advanced aircraft engines. When modifying processing and chemistry of disk alloys to achieve this capability, it is important to preserve the ability to use rapid cooling during supersolvus heat treatments to achieve coarse grain, fineγ′ microstructures. An important step in this effort is an understanding of the key variables controlling the cracking tendencies of nickel-base disk alloys during quenching from supersolvus heat treatments. The objective of this study was to investigate the quench cracking tendencies of several advanced disk superalloys during simulated heat treatments. Miniature disk specimens were rapidly quenched after solution heat treatments. The responses and failure modes were compared and related to the quench cracking tendencies of actual disk forgings. Cracking along grain boundaries was generally observed to be operative. For the alloys examined in this study, the solution temperature, not alloy chemistry, was found to be the primary factor controlling quench cracking. Alloys with high solvus temperatures show greater tendency for quench cracking.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.