Abstract

Objectives. To investigate pulpal space pressure and temperature after application of Nd:YAG laser, and high-speed diamond bur on dentin surface. Methods. One and 3 W Nd:YAG laser and high-speed diamond bur were used to remove dentine from twenty extracted premolars. The pulp chambers were monitored for pressure and temperature changes with a pressure transducer and thermocouple, respectively. Results. Regardless of the remaining dentin thickness (RDT), laser irradiation and high-speed diamond bur use generated an increase in pulpal space pressure and temperature (ANOVA and Fisher's LSD tests, P<0.001). Pressure and temperature increased with an increase in laser power. Three-Watt laser irradiation caused greater changes than 1 W (1.75 kPa and 1.31 °C, 0.53 kPa and 0.34 °C, respectively). Both pulpal space pressure ( P<0.001) and temperature ( P<0.005) increased as the RDT decreased. Conclusions. Laser irradiation and the use of a high-speed diamond bur generated an increase in pulpal space pressure and temperature. Pulpal space pressure and temperature increased with an increase in energy density of laser and a decrease in RDT.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.