ABSTRACT This article examines the development of water-swellable rubbers for oil and gas production packer equipment. The object of the investigation is to document the effect of rubber's acrylonitrile content on the swelling of the elastomers modified with sodium-carboxymethyl cellulose and a copolymer of acrylamide and potassium acrylate. After testing the samples at room temperature, the most influential factor in a material's swelling was discovered to be the mineral content in the liquids imitating well fluids. NBR polarity stemming from the inherent acrylonitrile (CN-group) level was not explicitly detected to affect the swelling rate and maximum ratio under the described conditions of the experiment. It was determined that in sodium chloride aqueous solutions with concentrations from 3 to 22%, swelling of nitrile rubber mostly depends on its cross-linking degree.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.