The conditions for obtaining and the rules for changing the color indices of ceramic pigments in the system CaO–MgO–Al2O3–SiO2–Cr2O3 are established. The main phase of such pigments is chromium garnet, formed with the direct participation of blast-furnace slag minerals. It is shown that as the acidity of pigment batches is increased by equimolecular substitution of free silicon dioxide in their composition based on phosphorus oxide (V) the purity and intensity of the green color of uvarovite pigments intensifies and the firing temperature of the pigments increases to 1100 – 1150°C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.