Abstract

Experimental data on molding of three-layered paperboard testliner from secondary fibre with an aerodynamically formed middle layer are presented. The layer-wise optimum ratios of low-quality fibres in the three-layered testliner with an aerodynamically formed middle layer for reducing paperboard production cost are given. The experimental data show the advantage of introduction of aerodynamic molding technology.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.