Abstract
Abstract Alumina/copper composites are used where high thermal conductivity, high absorption and dissipation of heat, high resistance to thermal fatigue and good frictional wear resistance are required. The properties of these composites depend on a number of factors including the content, shape and distribution of the ceramic phase, the method of their obtaining, as well as the conditions under which they are obtained. All these variables have influence on mentioned properties and, in consequence, on the future applications of the final material. The aim of this paper was to develop Cu-Al2O3 composites, processed using two techniques, namely sintering (of Cu /Al2O3 high-energy mixed powders) and tape casting (of slurry of the following composition: 1, 3 and 5 vol.% of Al2O3 phase; the remaining part: Cu). The compositions were determined taking into consideration the planned applications. The paper presents newly developed technologies, the results of both microstructure investigations as well as of the measurements of selected physical and mechanical properties (microhardness, wear resistance, thermal conductivity etc.) and contains the analysis of the influence of selected techniques and processing conditions on the properties and the interface morphology between ceramic and copper
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.