Abstract

Tungsten nitride film has been prepared by chemical vapor deposition using tungsten hexafluoride , ammonium, and hydrogen gas . film with metallic luster is obtained at 450°–600°C in the molar ratio of . Crystallite size of increases with increasing temperature from 450° to 650°C. SEM observation indicates that the size of particles in the film increases according to the change in crystallite size. ESCA spectra show that W‒N bond of has an ionic character, Wδ+ ‐ Nδ−.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.